Kinematic Viscosity at 40°C (104°F) 5.07 cSt
5.07 cSt
ASTM D 445
ConocoPhillips Hydroclear® 6 Ultra-Clean Spindle Oil
Description: Conoco Hydroclear Ultra-Clean Spindle fluids comprise blends of special base oils and additives specially formulated for use in applications where a lubricant combining the properties o..