Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 479 cSt | 479 cSt | ASTM D445 |
ChevronTexaco ParaMount™ ELV Paraffinic Process Oil FeaturesChevron ParaMount ELV Paraffinic Process Oil offers all the advantages of a bright stock including low weight loss and excellent solubility.ELV is exceptional because of its very light color.. |