Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 436 cSt | 436 cSt | ASTM D445 |
ExxonMobil Mobil Vaculine 546 Mobil Vacuoline 500 Series are extra high performance heavy duty circulating oils specifically designed to meet the critical requirements of the Morgan Construction Companys high speed No-Twist® Ro.. |
|||
Kinematic Viscosity at 40°C (104°F) | 436 cSt | 436 cSt | ASTM D445 |
ExxonMobil HH Mobil DTE Oil Double Letter Series The Mobil DTE Oil Double Letter Series of lubricants are high performance heavy duty circulating oils primarily intended for continuous reuse in circulation lubrication systems for gears and bearing.. |
|||
Kinematic Viscosity at 40°C (104°F) | 436 cSt | 436 cSt | ASTM D445 |
ExxonMobil Mobil Vaculine 546 Mobil Vacuoline 500 Series are extra high performance heavy duty circulating oils specifically designed to meet the critical requirements of the Morgan Construction Companys high speed No-Twist® Ro.. |
|||
Kinematic Viscosity at 40°C (104°F) | 436 cSt | 436 cSt | ASTM D445 |
ExxonMobil HH Mobil DTE Oil Double Letter Series The Mobil DTE Oil Double Letter Series of lubricants are high performance heavy duty circulating oils primarily intended for continuous reuse in circulation lubrication systems for gears and bearing.. |