Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 420 cSt
420 cSt
Base Oil
ConocoPhillips Syncon® Extra Long Life Grease NLGI No. 00
Description: Conoco Syncon Extra Long Life Grease is an ultra high performance lithium-complex grease with heavy synthetic base oil specifically designed for long service life under heavily loaded c..
Kinematic Viscosity at 40°C (104°F) 420 cSt
420 cSt
Base Oil
ConocoPhillips 1 Milube® Grease 2100 NLGI No. 1
Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic ..
Kinematic Viscosity at 40°C (104°F) 420 cSt
420 cSt
Base Oil
ConocoPhillips 1 Milube® Grease 2100T NLGI No. 1
Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic ..