Polymer Property : Kinematic Viscosity at 40°C (104°F) = 42.4 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 42.4 cSt
42.4 cSt
ASTM D445
ExxonMobil 846 Mobil DTE 800 Series
Mobil DTE 832 and 846 are superior performance turbine oils designed for use in steam turbines, gas turbines and combined cycle gas turbine (CCGT) applications under the most severe operating condit..
Kinematic Viscosity at 40°C (104°F) 42.4 cSt
42.4 cSt
ASTM D445
ExxonMobil 846 Mobil DTE 800 Series
Mobil DTE 832 and 846 are superior performance turbine oils designed for use in steam turbines, gas turbines and combined cycle gas turbine (CCGT) applications under the most severe operating condit..