Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 41.5 cSt | 41.5 cSt | ASTM D445 |
ExxonMobil Mobil Nyvac FR 200D Mobil Nyvac FR 200D is an extra high performance water-glycol type fire-resistant hydraulic fluid. It is formulated with diethylene glycol as the main glycol component. The product does not contain .. |
|||
Kinematic Viscosity at 40°C (104°F) | 41.5 cSt | 41.5 cSt | ASTM D445 |
ChevronTexaco ParaMount™ 2401 Paraffinic Process Oil FeaturesChevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content.Chevron’s modern all-hydroprocessing technology assur.. |
|||
Kinematic Viscosity at 40°C (104°F) | 41.5 cSt | 41.5 cSt | ASTM D445 |
ExxonMobil Mobil Nyvac FR 200D Mobil Nyvac FR 200D is an extra high performance water-glycol type fire-resistant hydraulic fluid. It is formulated with diethylene glycol as the main glycol component. The product does not contain .. |