Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 400 cSt | 400 cSt | Base Oil; ASTM D445 |
Nye Lubricants 783H (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 400 cSt | 400 cSt | Base Oil; ASTM D445 |
Nye Lubricants 824A-1 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 400 cSt | 400 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8190 (483) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 400 cSt | 400 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8192 (826-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 400 cSt | 400 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8192M (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 400 cSt | 400 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8192R (826RP-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 400 cSt | 400 cSt | Base Oil |
ConocoPhillips Tacna® HD Grease NLGI Grade 1 Tacna HD is a premium quality, adhesive, extreme-pressure (EP) lithium complex grease developed for the lubrication of heavily loaded construction, mining and industrial equipment. It also is recomm.. |
|||
Kinematic Viscosity at 40°C (104°F) | 400 cSt | 400 cSt | Base Oil |
ConocoPhillips Tacna® HD Grease NLGI Grade 2 Tacna HD is a premium quality, adhesive, extreme-pressure (EP) lithium complex grease developed for the lubrication of heavily loaded construction, mining and industrial equipment. It also is recomm.. |
|||
Kinematic Viscosity at 40°C (104°F) | 400 cSt | 400 cSt | ASTM D445 |
ChevronTexaco NLGI 2 Ultra Duty Grease EP FeaturesChevron Ultra-Duty Greases EP are versatile, multipurpose extreme pressure greases with high adhesive propertues designed for a wide variety of automotive and industrial applications.They ar.. |