Polymer Property : Kinematic Viscosity at 40°C (104°F) = 375 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 375 cSt
375 cSt
Base Oil; ASTM D445
Nye Lubricants 327A (SO) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 375 cSt
375 cSt
Base Oil; ASTM D445
Nye Lubricants 731 (IG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 375 cSt
375 cSt
ASTM D445
ExxonMobil 600 W Mobil Cylinder Oil
Mobil Cylinder oils are extra high performance high viscosity oils designed for use in enclosed worm gears operating at moderate to high speeds and temperatures, and where heavy loads, slow speeds o..
Kinematic Viscosity at 40°C (104°F) 375 cSt
375 cSt
ASTM D445
ExxonMobil 600 W Mobil Cylinder Oil
Mobil Cylinder oils are extra high performance high viscosity oils designed for use in enclosed worm gears operating at moderate to high speeds and temperatures, and where heavy loads, slow speeds o..