Polymer Property : Kinematic Viscosity at 40°C (104°F) = 3700 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 3700 cSt
3700 cSt
Base Oil; ASTM D445
Nye Lubricants 825F-1 (FG) Synthetic Oil
Information provided by Nye Lubricants.