Polymer Property : Kinematic Viscosity at 40°C (104°F) = 36.7 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 36.7 cSt
36.7 cSt
ChevronTexaco Cleartex® CF F
Texaco Cleartex CF metalworking fluid delivers value through:Multipurpose performance — Texaco Cleartex CF metalworking fluid is tri-purpose - serving as the cutting oil, hydraulic fluid, and machi..