Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 36.6 cSt | 36.6 cSt | |
ChevronTexaco Cleartex® CF D Texaco Cleartex CF metalworking fluid delivers value through:Multipurpose performance — Texaco Cleartex CF metalworking fluid is tri-purpose - serving as the cutting oil, hydraulic fluid, and machi.. |
|||
Kinematic Viscosity at 40°C (104°F) | 36.6 cSt | 36.6 cSt | |
Duratherm S Silicone Heat Transfer Fluid Duratherm S - a silicone based heat transfer fluid that is ideally suited for high oxidation or completely exposed systems up to 650°F. Duratherm S is virtually impervious to oxidation and offers s.. |