Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 36 cSt | 36 cSt | Base Oil; ASTM D445 |
Nye Lubricants 634B (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 36 cSt | 36 cSt | Base Oil; ASTM D445 |
Nye Lubricants 782G (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 36 cSt | 36 cSt | |
ExxonMobil Mobil ATF Type F Mobil ATF Type F is an automatic transmission fluid which is made from high quality base oils with viscosity index improvers, antioxidants, anti-wear agents, defoamants and special additives to prov.. |
|||
Kinematic Viscosity at 40°C (104°F) | 36 cSt | 36 cSt | |
ChevronTexaco Heavy Duty Synthetic Automatic Transmission Fluid Texaco Synthetic Automatic Transmission Fluid Heavy Duty delivers value through:Extended drains of up to four times that of a conventional automatic transmission fluid.Protection against the formati.. |
|||
Kinematic Viscosity at 40°C (104°F) | 36 cSt | 36 cSt | ASTM D445 |
ChevronTexaco Synthetic Automatic Transmission Fluid, Heavy Duty FeaturesChevron Synthetic Automatic Transmission Fluid Heavy Duty is engineered to meet the performance requirements of Allison TES 295 for severe duty and extended drain intervals. It is manufactu.. |
|||
Kinematic Viscosity at 40°C (104°F) | 36 cSt | 36 cSt | |
ChevronTexaco Transultex® CF F Texaco Transultex CF metalworking fluids deliver value through:Excellent antiweld properties from active sulfur and chlorine-free EP compounding which reduce frictional heat, prevent welding of meta.. |
|||
Kinematic Viscosity at 40°C (104°F) | 36 cSt | 36 cSt | ASTM D445 |
ChevronTexaco Superla® 18 White Oil FeaturesChevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F.These nearly ch.. |
|||
Kinematic Viscosity at 40°C (104°F) | 36 cSt | 36 cSt | |
ExxonMobil Mobil ATF Type F Mobil ATF Type F is an automatic transmission fluid which is made from high quality base oils with viscosity index improvers, antioxidants, anti-wear agents, defoamants and special additives to prov.. |