Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 34.2 cSt | 34.2 cSt | ASTM D445 |
ExxonMobil 32 Mobil EAL Arctic Series Mobil EAL Arctic Series are high performance Environmental Awareness Lubricants (EAL) that are fully synthetic products designed specifically for the lubrication of refrigeration compressors and sys.. |
|||
Kinematic Viscosity at 40°C (104°F) | 34.2 cSt | 34.2 cSt | ASTM D445 |
ExxonMobil 32 Mobil EAL Arctic Series Mobil EAL Arctic Series are high performance Environmental Awareness Lubricants (EAL) that are fully synthetic products designed specifically for the lubrication of refrigeration compressors and sys.. |
|||
Kinematic Viscosity at 40°C (104°F) | 34.2 cSt | 34.2 cSt | |
ELM® SoyFluid™ Hydraulic All Season Premium Biodegradable - Biobased Hydraulic Oil Description: ELM Biotechbased SoyFluid Hydraulic All Season Oil is a biodegradable hydraulic oil formulated with the best optimized USA grown natural seed oils that surpass the lubricity of most con.. |