Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 180 (SO) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 180A (SO) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 180P (SO) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 362F (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 362HF (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 362HF-UV (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 362HM (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 362HT (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 373 (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 375 (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 723G (RL) Rheolube Grease
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 723MS (RL) Rheolube Grease
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 723S-MS (RL) Rheolube Grease
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 723TF (RL) Rheolube Grease
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 725A (RL) Rheolube Grease
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 734B (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 744 (NG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 744F-MS (NG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 744-UV (NG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants 757SSG (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8961 (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8961F (896-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8961R (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8961UF (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
ConocoPhillips Conoflex® 32 SRI Lubricant ISO
Description: Conoco Conoflex SRI Lubricant is an excellent wire rope lubricant and preservative for any metal product, particularly when protecting from saltwater. It lubricates and preserves the wi..
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
ConocoPhillips Hydroclear® MV32 AW Hydraulic Fluid
Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a..
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
ConocoPhillips Hydroclear® 32 TCS Slideway lubricant
Description: Conoco Hydroclear® TCS Slideway Lubricant is a premium demulsible machine tool way lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear TCS Slideway Lubricant ..
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
ConocoPhillips Hydroclear® Automatic Transmission Fluid
Description: Conoco Hydroclear DEXRON® III & MERCON® Automatic Transmission Fluid is a multipurpose fluid for the electronically controlled transmissions of most domestic and imported automobiles,..