Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 327 cSt | 327 cSt | ASTM D-445 |
ConocoPhillips ANDEROL® PQ AA 85W140 White Mineral Food Grade Gear Oil, ISO Grade 320, SAE Gear Oil Grade 85W140 Description: ANDEROL PQ AA Series Gear Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Gear.. |