Polymer Property : Kinematic Viscosity at 40°C (104°F) = 3200 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 3200 cSt
3200 cSt
Base Oil; ASTM D445
Nye Lubricants 876M-MS FG) Grease
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 3200 cSt
3200 cSt
ChevronTexaco Meropa® 3200
Texaco Meropa oils deliver value through:Gear set efficiencies — High thermal stability EP system maintains clean gear and bearing surfaces, minimizing deposits which interfere with effective lubri..