Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Kinematic Viscosity at 40°C (104°F) = 32.4 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 32.4 cSt
32.4 cSt
ASTM D445
ExxonMobil 624 Mobil SHC 600 Series
Mobil SHC 600 Series lubricants are good performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are for..
Kinematic Viscosity at 40°C (104°F) 32.4 cSt
32.4 cSt
ChevronTexaco Biostar® Hydraulic 32
Texaco Biostar Hydraulic oils deliver value through:Environmental sensitivity — Readily biodegradable formulation supports use in environmentally sensitive applications.Reduced maintenance — Ashle..
Kinematic Viscosity at 40°C (104°F) 32.4 cSt
32.4 cSt
ASTM D445
ExxonMobil 624 Mobil SHC 600 Series
Mobil SHC 600 Series lubricants are good performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are for..