Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 30.6 cSt | 30.6 cSt | ASTM D445 |
ExxonMobil Mobiltherm 43 Mobiltherm 43 is a formulated paraffinic type fluid designed for closed heat transfer systems operating at higher bulk temperatures including demanding open systems. It has a high specific heat an.. |
|||
Kinematic Viscosity at 40°C (104°F) | 30.6 cSt | 30.6 cSt | ASTM D445 |
ExxonMobil Mobiltherm 43 Mobiltherm 43 is a formulated paraffinic type fluid designed for closed heat transfer systems operating at higher bulk temperatures including demanding open systems. It has a high specific heat an.. |