Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 3.9 cSt | 3.9 cSt | |
ChevronTexaco EDM Fluid Texaco EDM Fluid delivers value through:Accurate machining — Good dielectric properties provide controlled discharge characteristics. Low viscosity provides excellent fluidity through the spark gap.. |