Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 290 cSt | 290 cSt | See Note 3. |
ChevronTexaco Marfak® Heavy Duty 2 Texaco Marfak grease delivers value through:Good film strengthGood rust and corrosion protection, even in wet conditions.Texaco Marfak greases are fibrous sodium soap greases. It resists oil separat.. |
|||
Kinematic Viscosity at 40°C (104°F) | 290 cSt | 290 cSt | See Note 3. |
ChevronTexaco Marfak® Heavy Duty 3 Texaco Marfak grease delivers value through:Good film strengthGood rust and corrosion protection, even in wet conditions.Texaco Marfak greases are fibrous sodium soap greases. It resists oil separat.. |