Polymer Property : Kinematic Viscosity at 40°C (104°F) = 29.3 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 29.3 cSt
29.3 cSt
ASTM D445
ExxonMobil Mobilgrease 28
Mobilgrease 28 is a supreme performance, wide-temperature, antiwear grease designed to combine the unique features of a polyalphaolefin (PAO) synthetic base fluid with an organo-clay (non-soap) thic..
Kinematic Viscosity at 40°C (104°F) 29.3 cSt
29.3 cSt
ASTM D445
ExxonMobil Mobilgrease 28
Mobilgrease 28 is a supreme performance, wide-temperature, antiwear grease designed to combine the unique features of a polyalphaolefin (PAO) synthetic base fluid with an organo-clay (non-soap) thic..