Polymer Property : Kinematic Viscosity at 40°C (104°F) = 28.9 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 28.9 cSt
28.9 cSt
ASTM D445
ChevronTexaco Elite-Cut® AD Metal Working Fluid
FeaturesChevron -Cut Metalworking Fluids are a complete line of chlorinated cutting oils. The line consists of individual products with antiweld and lubricity properties to cover practically all met..