Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 27.8 cSt @Temperature 40.0 °C |
27.8 cSt @Temperature 104 °F |
ASTM D445 |
PolyOne Synplast™ DINP-N Di Isononyl Phthalate Branched C9 phthalate esterInformation provided by PolyOne |