Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 255 cSt | 255 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8180 (479) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 255 cSt | 255 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8182 (837) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 255 cSt | 255 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8182R (837RP) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 255 cSt | 255 cSt | |
ChevronTexaco 120 Aircraft Engine Oils Premium AD Texaco Aircraft Engine Oils Premium AD deliver value through:Clean engines due to the dispersancy action. Minimal deposits in the combustion chamber, spark plugs, rings, valves, etc.Low wear — Maxi.. |