Polymer Property : Kinematic Viscosity at 40°C (104°F) = 25000 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 25000 cSt
25000 cSt
Base Oil; ASTM D445
Nye Lubricants 783D (NG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 25000 cSt
25000 cSt
Base Oil; ASTM D445
Nye Lubricants 910 (NG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 25000 cSt
25000 cSt
Base Oil; ASTM D445
Nye Lubricants 783DB (NG) Synthetic Oil
Information provided by Nye Lubricants.