Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 23 cSt
23 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8310 (472) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 23 cSt
23 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8311 (833-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 23 cSt
23 cSt
Base Oil; ASTM D445
Nye Lubricants 833Z-1 (FG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 23 cSt
23 cSt
ConocoPhillips MV22 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Kinematic Viscosity at 40°C (104°F) 23 cSt
23 cSt
Lubriplate MAG-00 Lithium-Polymer Type Grease For Special Applications / Conditions
These multi-purpose, lithium polymer greases have a wide operating temperature range for a variety of applications from -60°F to 300°F. Applications: Centralized systems, leaking gearboxes. MAG-00..
Kinematic Viscosity at 40°C (104°F) 23 cSt
23 cSt
Lubriplate MAG-1 Lithium-Polymer Type Grease For Special Applications / Conditions
These multi-purpose, lithium polymer greases have a wide operating temperature range for a variety of applications from -60°F to 300°F. Applications: Cold and wide temp. range, multi-purpose.MAG-1..