Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 228 cSt
228 cSt
ASTM D445
ExxonMobil 100 Exxon Aviation Oil
Aviation Oil 100, 120 and 20W-50 are  non-dispersant, mineral oil-based lubricants for piston engines of commercial, military and private aircraft. They contain very low concentrations of anti-oxid..
Kinematic Viscosity at 40°C (104°F) 228 cSt
228 cSt
ASTM D445
ExxonMobil 100 Exxon Aviation Oil
Aviation Oil 100, 120 and 20W-50 are  non-dispersant, mineral oil-based lubricants for piston engines of commercial, military and private aircraft. They contain very low concentrations of anti-oxid..