Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 225 cSt | 225 cSt | ASTM D445 |
ExxonMobil 220 Mobil SHC PM Series Mobil SHC PM Series products are supreme performance synthetic lubricants specifically designed for the most demanding industrial paper machine circulating systems. They are engineered to provide ex.. |
|||
Kinematic Viscosity at 40°C (104°F) | 225 cSt | 225 cSt | ASTM D445 |
ChevronTexaco Delo® 400 SAE 50 Chevron Delo 400 heavy duty motor oils are exceptional, super premium quality “universal” engine oils which exceed industry and engine manufacturers’ performance requirements.They are formulated .. |
|||
Kinematic Viscosity at 40°C (104°F) | 225 cSt | 225 cSt | ASTM D445 |
ExxonMobil 220 Mobil SHC PM Series Mobil SHC PM Series products are supreme performance synthetic lubricants specifically designed for the most demanding industrial paper machine circulating systems. They are engineered to provide ex.. |