Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 22000 cSt | 22000 cSt | Base Oil; ASTM D445 |
Nye Lubricants 823A-1 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 22000 cSt | 22000 cSt | ASTM D445 |
ExxonMobil 22M Mobilgear SHC Mobilgear SHC 22M and 46M are supreme performance ultra high viscosity synthetic lubricants designed specifically for use in heavily loaded, low speed gears where boundary lubrication conditions oft.. |
|||
Kinematic Viscosity at 40°C (104°F) | 22000 cSt | 22000 cSt | ASTM D445 |
ExxonMobil 22M Mobilgear SHC Mobilgear SHC 22M and 46M are supreme performance ultra high viscosity synthetic lubricants designed specifically for use in heavily loaded, low speed gears where boundary lubrication conditions oft.. |