Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 213 cSt | 213 cSt | |
ChevronTexaco Taro® 16 XD SAE 50 Texaco Taro 16 XD delivers value through:Wear protection — Superior antiwear characteristics result in reduced wear on all moving engine components. Controls ring and liner wear through its ability.. |