Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 20.2 cSt | 20.2 cSt | ASTM D445 |
ExxonMobil 603 Mobiltherm 600 Series Mobiltherm heat transfer oils are high performance products intended for use in closed indirect heating installations. They are formulated from highly refined base stocks that are resistant to therm.. |
|||
Kinematic Viscosity at 40°C (104°F) | 20.2 cSt | 20.2 cSt | |
ChevronTexaco Quenchtex® A Texaco Quenchtex oils deliver value through:Controlled cooling of metals — Combines the high initial quenching speed of water with slow final quenching speed of oil.Safety — High flash point and f.. |
|||
Kinematic Viscosity at 40°C (104°F) | 20.2 cSt | 20.2 cSt | ASTM D445 |
ExxonMobil 603 Mobiltherm 600 Series Mobiltherm heat transfer oils are high performance products intended for use in closed indirect heating installations. They are formulated from highly refined base stocks that are resistant to therm.. |