Polymer Property : Kinematic Viscosity at 40°C (104°F) = 190 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 190 cSt
190 cSt
Base Oil
ConocoPhillips SUPER-STA NLGI No. 1
Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C...
Kinematic Viscosity at 40°C (104°F) 190 cSt
190 cSt
Base Oil
ConocoPhillips SUPER-STA NLGI No. 2
Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C...
Kinematic Viscosity at 40°C (104°F) 190 cSt
190 cSt
Base Oil
ConocoPhillips EP Conolith® Grease NLGI NO. 0
Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th..
Kinematic Viscosity at 40°C (104°F) 190 cSt
190 cSt
Base Oil
ConocoPhillips EP Conolith® Grease NLGI NO. 00
Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th..
Kinematic Viscosity at 40°C (104°F) 190 cSt
190 cSt
Base Oil
ConocoPhillips EP Conolith® Grease NLGI NO. 000
Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th..
Kinematic Viscosity at 40°C (104°F) 190 cSt
190 cSt
Base Oil
ConocoPhillips EP Conolith® Grease NLGI NO. 1
Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th..
Kinematic Viscosity at 40°C (104°F) 190 cSt
190 cSt
Base Oil
ConocoPhillips EP Conolith® Grease NLGI NO. 2
Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th..
Kinematic Viscosity at 40°C (104°F) 190 cSt
190 cSt
Base Oil
ConocoPhillips SUPER-STA M NLGI No.0
Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C...
Kinematic Viscosity at 40°C (104°F) 190 cSt
190 cSt
Base Oil
ConocoPhillips SUPER-STA M NLGI No.2
Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C...
Kinematic Viscosity at 40°C (104°F) 190 cSt
190 cSt
Base Oil
ConocoPhillips SUPER-STA M NLGI No.1
Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C...