Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 159.7 cSt | 159.7 cSt | ASTM D445 |
ChevronTexaco ECO® SAE 40 Heavy Duty Motor Oil Features:Chevron ECO Heavy Duty Motor Oils are formulated to be environmentally responsible engine lubricants. They use the highest quality re-refined base oils and specially selected additives desi.. |