Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 14.3 cSt | 14.3 cSt | ASTM D445 |
ChevronTexaco ISO 15 Handy Oil FeaturesChevron Handy Oil is a highly refined, light-bodied, multipurpose lubricating oil.It contains an oxidation inhibitor to improve its natural stability and prevent the formation of gums and va.. |