Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 139 cSt | 139 cSt | ASTM D445 |
ExxonMobil HD Plus 80W-90 Mobilube HD Plus 80W-90 and 85W-140 are extra high performance commercial gear lubricants formulated from select base oils and an advanced additive system. These lubricants are engineered for perfor.. |
|||
Kinematic Viscosity at 40°C (104°F) | 139 cSt | 139 cSt | ASTM D445 |
ExxonMobil HD Plus 80W-90 Mobilube HD Plus 80W-90 and 85W-140 are extra high performance commercial gear lubricants formulated from select base oils and an advanced additive system. These lubricants are engineered for perfor.. |