Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 133 cSt | 133 cSt | ASTM D445 |
ChevronTexaco RPM® SAE 50 Synthetic Transmission Fluid FeaturesChevron RPM Synthetic Transmission Fluid is a heavy duty truck manual transmission fluid.It is manufactured from synthesized hydrocarbon base fluids which have excellent thermal and oxidatio.. |
|||
Kinematic Viscosity at 40°C (104°F) | 133 cSt | 133 cSt | |
ChevronTexaco Syn-Star® TL SAE 50 Texaco Syn-Star® TL delivers value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oil used in this product provides outstanding stability.Extended drain capabil.. |
|||
Kinematic Viscosity at 40°C (104°F) | 133 cSt | 133 cSt | |
ConocoPhillips Conoco® El Mar® Geo Low Ash Oil, SAE Viscosity Grade 40 Conoco® El Mar GEO Oil is a high-quality, non-detergent, ashless gas engine oil designed primarily for use in Ajax 2-stroke cycle natural gas engines. The SAE 15W-40 viscosity grade meets the low-t.. |
|||
Kinematic Viscosity at 40°C (104°F) | 133 cSt | 133 cSt | |
ConocoPhillips Conoco® El Mar® Geo Low Ash Oil, SAE Viscosity Grade 30 Conoco® El Mar GEO Oil is a high-quality, non-detergent, ashless gas engine oil designed primarily for use in Ajax 2-stroke cycle natural gas engines. The SAE 15W-40 viscosity grade meets the low-t.. |