Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 13.2 cSt | 13.2 cSt | ASTM D445 |
ChevronTexaco AFP White Oil Chevron White Oil AFP is a technical grade white oil processed from paraffinic oilApplicationsChevron White Oil AFP’s major application is the dedusting of animal feeds and the preparation of anima.. |