Polymer Property : Kinematic Viscosity at 40°C (104°F) = 129 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 129 cSt
129 cSt
ConocoPhillips Syncon® 15W-50 High Performance Synthetic Motor Oil
Description: Conoco Syncon HP Synthetic Motor Oil is formulated for most domestic or imported vehicles with gasoline-powered engines. It works well at extreme temperatures and in severe driving cond..
Kinematic Viscosity at 40°C (104°F) 129 cSt
129 cSt
See Note 3.
ChevronTexaco PremiumRB
Texaco Premium RB delivers value through:Wide application range — Suitable for high rpm operation, operating temperatures ranging from -34°C to 177°C (-30°F to 350°F) and offers excellent rust ..
Kinematic Viscosity at 40°C (104°F) 129 cSt
129 cSt
ConocoPhillips Hydroclear® El Mar® 40 Ashless Supreme
Description: Conoco Hydroclear El Mar Ashless Supreme is a premium ashless natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Ashless Supreme is speci..