Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 1240 cSt
1240 cSt
ASTM D445
ExxonMobil SpectraSyn™ 100 Polyalphaolefin (PAO) Fluid
Product Description: SpectraSyn™ High Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties (pour point and viscosity), low volatility, and improved thermal stability. Spect..