Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 121 cSt | 121 cSt | Base Oil; ASTM D445 |
Nye Lubricants 374A (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 121 cSt | 121 cSt | ASTM D445 |
ExxonMobil Mobil Pegasus 710 40 Mobil Pegasus 710 is a premium performance gas engine oil primarily intended for the lubrication of modern high-speed four-cycle engines where oil consumption is very low. These engines are generall.. |
|||
Kinematic Viscosity at 40°C (104°F) | 121 cSt | 121 cSt | ASTM D445 |
ExxonMobil Mobil Pegasus 710 40 Mobil Pegasus 710 is a premium performance gas engine oil primarily intended for the lubrication of modern high-speed four-cycle engines where oil consumption is very low. These engines are generall.. |