Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 116 cSt | 116 cSt | ASTM D445 |
ChevronTexaco 600R Neutral Oil FeaturesChevron Neutral Oils are all-hydroprocessed, highly refined API Group II paraffinic base stocks. Their extremely low sulfur, nitrogen, and aromatic content give them excellent thermal and o.. |
|||
Kinematic Viscosity at 40°C (104°F) | 116 cSt | 116 cSt | ASTM D445 |
ChevronTexaco 60-T White Oil FeaturesChevron White Oils are technical grade oils processed from paraffinic oil. Mixtures of paraffinic and naphthenic hydrocarbons, they are virtually free of nitrogen, sulfur, oxygen, and aroma.. |
|||
Kinematic Viscosity at 40°C (104°F) | 116 cSt | 116 cSt | ASTM D445 |
ChevronTexaco Delo® 400 Multigrade, SAE 15W-40 Features:Chevron Delo 400 Multigrade heavy duty motor oil is a super premium quality "universal" engine oil which exceeds industry and engine manufacturers performance requirements. It is formulated.. |
|||
Kinematic Viscosity at 40°C (104°F) | 116 cSt | 116 cSt | ASTM D445 |
ChevronTexaco ParaLux® 6001R Process Oil FeaturesPARALUX is produced using an all-hydroprocessing route which transforms the molecular structure of undesirable aromatics into highly desirable saturates. This produces a process oil with sup.. |
|||
Kinematic Viscosity at 40°C (104°F) | 116 cSt | 116 cSt | ASTM D445 |
ChevronTexaco ParaLux™ 6001 Paraffinic Process Oil FeaturesPARALUX is produced using an all-hydroprocessing route which transforms the molecular structure of undesirable aromatics into highly desirable saturates. This produces a process oil with sup.. |
|||
Kinematic Viscosity at 40°C (104°F) | 116 cSt | 116 cSt | See Note 3. |
ChevronTexaco Polystar® RB NLGI Grade 2 Texaco Polystar RB 2 delivers value through:Ability to meet bearing OEM requirements — Suitable for high rpm operations, operating temperatures ranging from -34°C to 204°C (-30°F to 400°F) and .. |
|||
Kinematic Viscosity at 40°C (104°F) | 116 cSt | 116 cSt | ASTM D445 |
ChevronTexaco RPM® SAE 15W-40 Heavy Duty Motor Oil Features: Chevron RPM Heavy Duty Motor Oils are premium quality, mixed fleet motor oils meeting the performance requirements of all four-stroke gasoline engines and all naturally aspirated, turbocha.. |
|||
Kinematic Viscosity at 40°C (104°F) | 116 cSt | 116 cSt | |
ChevronTexaco URSA® SAE 15W-40 Super Plus Texaco Ursa Super Plus SAE 15W-40 delivers value through:One oil for all services, both diesel and gasoline, minimizes the chance of misapplication.educed inventory investment — No need to maintain.. |
|||
Kinematic Viscosity at 40°C (104°F) | 116 cSt | 116 cSt | |
ConocoPhillips HD Fleet Supreme™ 15W-40 Engine Oil Description: Conoco HD Fleet Supreme Engine Oil is a high-quality engine oil formulated from Conoco's premium hydrocracked base stock and unique additive technology. It easily satisfies the warr.. |
|||
Kinematic Viscosity at 40°C (104°F) | 116 cSt | 116 cSt | |
ConocoPhillips Hydroclear® 580 Industrial Oil Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommende.. |
|||
Kinematic Viscosity at 40°C (104°F) | 116 cSt | 116 cSt | ASTM D445 |
ChevronTexaco NLGI 2 SRI Grease FeaturesChevron SRI Grease is a high temperature ball and roller bearing grease.It is formulated with ISOSYN® base stocks, a synthetic polyurea ashless organic thickener, and high performance rust .. |