Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 114.1 cSt | 114.1 cSt | ASTM D445 |
ChevronTexaco 600 White Oil FeaturesChevron Technical White Oils are high quality, highly refined, odorless, tasteless, clear, paraffinic, technical grade white oils.Chevron Technical White Oils are hydrocracked and dewaxed us.. |