Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 11.6 cSt @Temperature 40.0 °C |
11.6 cSt @Temperature 104 °F |
ASTM D445 |
PolyOne Synplast™ DOS-N Di (2-ethylhexyl) Sebacate Branched C8 sebacate esterInformation provided by PolyOne |