Polymer Property : Kinematic Viscosity at 40°C (104°F) = 11 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 11 cSt
11 cSt
Base Oil; ASTM D445
Nye Lubricants 856 (FG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 11 cSt
11 cSt
ConocoPhillips Hydroclear® 70 Industrial Oil
Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommende..