Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 106 cSt | 106 cSt | ASTM D445 |
ChevronTexaco MP Drive Train Fluid FeaturesChevron Drive Train Fluid - MP is a multipurpose lubricant designed for use in transmissions, wet brakes, and hydraulic systems requiring a fluid meeting Caterpillar TO-4 or TO-4M requiremen.. |
|||
Kinematic Viscosity at 40°C (104°F) | 106 cSt | 106 cSt | ASTM D445 |
ChevronTexaco Tool Joint Compound FeaturesChevron Tool Joint Compound is an aluminum complex grease designed principally for the lubrication of drill collars, tool joints and pipe threads.It contains copper flake and graphite, forti.. |
|||
Kinematic Viscosity at 40°C (104°F) | 106 cSt | 106 cSt | |
ChevronTexaco URSA® SAE 15W-40 Premium TDX Texaco Ursa Premium TDX SAE 15W-40 delivers value through:Reduced wear — Prolonging component life and providing reduced maintenance costs.Improved engine cleanliness — Providing efficient operati.. |
|||
Kinematic Viscosity at 40°C (104°F) | 106 cSt | 106 cSt | |
ConocoPhillips Conoco® El Mar® Ashless Supreme Oil, SAE Viscosity Grade 15W-40 Conoco® El Mar Ashless Supreme is a premium quality, ashless, dispersant-detergent gas engine oil designed for use in naturally aspirated and turbocharged 2-stroke cycle natural gas engines. Engine.. |
|||
Kinematic Viscosity at 40°C (104°F) | 106 cSt | 106 cSt | ASTM D445 |
ChevronTexaco Delo® 2000 Marine Engine Oil, SAE 30 FeaturesChevron Marine Engine Oil Delo 2000 Marine is a high quality engine oil developed for use in a wide variety of medium speed trunk piston engines burning marine diesel oils, or residual fuels.. |
|||
Kinematic Viscosity at 40°C (104°F) | 106 cSt | 106 cSt | ASTM D445 |
ExxonMobil Mobil 1 75W-90 Gear Lubricant LS Mobil 1 Synthetic Gear Lubricant LS is a supreme performance, synthetic, multi-purpose, SAE 75W-90 automotive gear lubricant designed to meet the highest level performance requirements of modern pas.. |
|||
Kinematic Viscosity at 40°C (104°F) | 106 cSt | 106 cSt | ASTM D445 |
ExxonMobil Mobil 1 75W-90 Gear Lubricant LS Mobil 1 Synthetic Gear Lubricant LS is a supreme performance, synthetic, multi-purpose, SAE 75W-90 automotive gear lubricant designed to meet the highest level performance requirements of modern pas.. |