Polymer Property : Kinematic Viscosity at 40°C (104°F) = 104.6 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 104.6 cSt
104.6 cSt
ASTM D445
ExxonMobil Mobil Rarus 427
The Mobil Rarus 400 Series is a line of premium performance ashless air compressor lubricants designed to meet the stringent requirements of the major compressor manufacturers. They are formulated w..
Kinematic Viscosity at 40°C (104°F) 104.6 cSt
104.6 cSt
ASTM D445
ExxonMobil Mobil Rarus 427
The Mobil Rarus 400 Series is a line of premium performance ashless air compressor lubricants designed to meet the stringent requirements of the major compressor manufacturers. They are formulated w..
Kinematic Viscosity at 40°C (104°F) 104.6 cSt
104.6 cSt
Base Oil; ASTM D445
Nye Lubricants 2001T (SO) Synthetic Oil
Information provided by Nye Lubricants.