Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 10.7 cSt @Temperature 40.0 °C |
10.7 cSt @Temperature 104 °F |
ASTM D445 |
PolyOne Synplast™ DINA-N Di Isononyl Adipate Branched C9 adipate esterInformation provided by PolyOne |