Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 10.3 cSt @Temperature 40.0 °C |
10.3 cSt @Temperature 104 °F |
ASTM D445 |
PolyOne Synplast™ DOZ-E Di (2-ethylhexyl) Azelate Branched C8 azelate ester with antioxidantContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |
|||
Kinematic Viscosity at 40°C (104°F) | 10.3 cSt | 10.3 cSt | ASTM D445 |
ExxonMobil 762 Mobilmet 760 Series Mobilmet 760 Series are extra high performance oil based cutting oils. They are chlorine-free and are intended for severe cutting operations especially on difficult to machine steels. They are corro.. |
|||
Kinematic Viscosity at 40°C (104°F) | 10.3 cSt | 10.3 cSt | ASTM D445 |
ChevronTexaco ISO 10 Hydraulic Oil AW FeaturesChevron Hydraulic Oils AW are designed to give excellent hydraulic pump protection. They are formulated with refined paraffinic base oils. They provide excellent antiwear protection, oxidati.. |
|||
Kinematic Viscosity at 40°C (104°F) | 10.3 cSt | 10.3 cSt | ASTM D445 |
ExxonMobil 762 Mobilmet 760 Series Mobilmet 760 Series are extra high performance oil based cutting oils. They are chlorine-free and are intended for severe cutting operations especially on difficult to machine steels. They are corro.. |
|||
Kinematic Viscosity at 40°C (104°F) | 10.3 cSt | 10.3 cSt | |
ChevronTexaco Spindura® 10 Texaco Spindura oils deliver value through:High oxidation stability — Longer service life than with conventional lubricants.Rust and corrosion protection — Gives excellent protection against corro.. |