Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 7.0 cSt | 7.0 cSt | |
Lubriplate 68-N Naphthenic Refrigeration Compressor Oil These highly refined lubricants are formulated for use in refrigeration compressor systems utilizing ammonia, CFC (chlorofluorocarbon) and HCFC (hydrochlorofluorocarbon) refrigerants such as R-717, .. |
|||
Kinematic Viscosity at 100°C (212°F) | 7.0 cSt | 7.0 cSt | |
Lubriplate AC-1 Petroleum-Based Air Compressor Fluid Formulated to reduce carbon & varnish buildup. They contain fluid zinc to effectively fight friction & wear thus reducing heat & foaming. Available in six ISO grades.AC Series Air Compressor Oils ar.. |
|||
Kinematic Viscosity at 100°C (212°F) | 7.0 cSt | 7.0 cSt | |
Lubriplate H0-1 Petroleum-Based Heavy-Duty Hydraulic Oil Formulated for superior performance, this series contains fluid zinc to effectively reduce ring & vane wear. Excellent anti-rust, anti-corrosion, anti-foam and anti-oxidation properties. High anilin.. |
|||
Kinematic Viscosity at 100°C (212°F) | 7.0 cSt | 7.0 cSt | |
Lubriplate Low Pour Petroleum-Based Heavy-Duty Hydraulic Oil ISO 22 petroleum-based oil for low temperature applications. Low Temp Hydraulic Oils are available in Jugs, Pails, 1/4 Drums & Drums.Information provided by Lubriplate |
|||
Kinematic Viscosity at 100°C (212°F) | 7.0 cSt | 7.0 cSt | |
Lubriplate SYNAC 46 Diester-Based Synthetic Air Compressor Fluid These diester-based synthetic air compressor fluids are outstanding for applications where the fluid is subjected to high temperature and high stress conditions over extended drain intervals.Synac S.. |