Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 45 cSt | 45 cSt | |
Lubriplate SFGO Ultra-460 PAO-Based Synthetic Food Machinery Grade Fluid Polyalphaolefin (PAO)-based high-performance fluids formulated with 100% PAO synthetic base fluids for a variety of demanding applications. They are outstanding lubricants for use under severe condi.. |
|||
Kinematic Viscosity at 100°C (212°F) | 45 cSt | 45 cSt | ASTM D445 |
Solvay Specialty Polymers FOMBLIN® M30 PFPE Lubricant Information provided by Solvay Solexis, Inc. |